Taylor-White process
5 syllables, stress on the first, lighter stress on the fourth
A process (invented about 1899 by Frederick W. Taylor and Maunsel B. White) for giving toughness to self-hardening steels. The steel is heated almost to fusion, cooled to a temperature of from 700º to 850º C. in molten lead, further cooled in oil, reheated to between 370º and 670º C., and cooled in air.